TPR、TPR脚轮料、惠州TPR胶料供应商(智能穿戴) TPR材料RN35D-01
TPE制品加工色差是注塑中常见的缺陷, 因配套件颜色差别造成注塑机成批报废的情况并不小见。色差影响因素众多,涉及原料树脂、色母、色母同原料的混合、注塑工艺、注塑机、模具等,正因为牵涉面广泛,因此色差控制技术同时也是注塑中公认较难掌握技术之一。在实际的生产过程中我们一般从以下六个方面来进行色差的控制。
1.消除注塑机及模具因素的影响
要选择与注塑主品容量相当的注塑机,如果注塑机存在物料死角等问题,最好更换设备。对于模具浇注系统、排气槽等造成色差的,可通过相应部分模具的维修模来解决。必须首先解决好注塑机及模具问题才可以组织生产,以削减问题的复杂性。
产品说明Product description |
||||||||
·RN35D-01是一款高性能材料,具有良好的抗冲击和抗疲劳性能。 ·RN35D-01 is a kind of high performance material which has excellent impact resistance and fatigue resistance properties. |
||||||||
关键特性Key characteristic |
||||||||
1.表面光亮Bright surface. 2..可喷油,丝印,上胶水,油墨Oil injection,silkscreen,can be applied with glue and ink. 3.弹性优良,易成型Excellent elasticity,easy molding. |
||||||||
功能Function |
||||||||
产品应用 Main application |
玩具公仔Toy dolls |
运动器材Sports equipment |
||||||
鞋材 Shoe material |
|
|||||||
加工方法Processing method |
注塑成型Injection molding |
|||||||
环保认证 Environmental certification |
ROHS |
REACH |
EN71-3 |
|||||
PAHS |
ASTM-F963 |
Phthalate |
||||||
颜色Color |
乳白色Milky-white |
|||||||
气味Smell |
少许树脂味A little resin smell |
|||||||
外型Appearance |
圆球形小颗粒Cylindrical particle,about 3mm×1.5mm |
|||||||
储藏期Storage period |
常温下通风干燥,12个月Ventilated dry at normal temperature,about 12 months |
|||||||
包装方式Packaging method |
25公斤/袋 25kg/bag |
|||||||
物理性能Physical properties |
结果Result |
单位Unit |
方法Method |
成型条件Molding condition |
||||
比重Specific gravity |
0.9±0.02 |
g/cm3 |
ASTM D792 |
干燥温度Drying temp |
||||
硬度Hardness |
35±5 |
shoreA |
ASTM D2240 |
干燥时间Drying time |
||||
拉伸强度Tensile strength |
>3 |
Mpa |
ASTM D412 |
射嘴温度Nozzle temp 180℃ |
||||
断裂延伸Elongation at break |
>500 |
% |
ASTM D412 |
螺筒一段温度Screw 1 temp 170℃ |
||||
撕裂强度Tearing strength |
>9 |
Kn/m |
ASTM D624 |
螺筒二段温度Screw 2 temp 160℃ |
||||
熔融指数Melt index |
>25 |
g/10min |
ASTM D1238 |
螺筒三段温度Screw 3 temp 150℃ |
||||
注意事项Matters need attention |
||||||||
清洗料管 Purge compound |
需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean. |
|||||||
着色 Coloring
|
请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed are backpressure are needed for better colorant dispersion. |
|||||||
回收 Recycling |
二次料(水口料)回收比率建议最多20%. Consistent regrind usage of up to 20% is permissible. |