厂家新品 TPE原料 TPR颗粒 注塑级 公仔 玩具

ES35F-01是一款高回弹性透明材料,具有极好的耐刮擦性和耐候性。 ·ES35F-01 is a kind of high resilience and translucent material which has excellent scratch resistance and weather resistance properties.
  • 产品描述
  • 倍韧/BESTPERNE®ES35F-01

    热塑性弹性体Thermoplastic Elastomer

    产品说明Product description

    ·ES35F-01是一款高回弹性透明材料,具有极好的耐刮擦性和耐候性

    ·ES35F-01 is a kind of high resilience and translucent material which has excellent scratch resistance and weather resistance properties.

    关键特性Key characteristic

    1. 耐老化性优良,不易黄变excellent ageing resistance and not easy to yellowing
    2. 表面哑,手感柔软干爽。dumb surface,soft and dry touch
    3. 模量高,不易变形high modulus,not easy to deformation
    4. 成型快,不粘模具rapid molding,non-stick mold

    功能Function

    产品应用

    Main application

    玩具产品Toy products

    挤出管  Extruded tube

    H运动器材HSports equipment

     

    加工方法Processing method

     注塑成型Injection molding     挤出成型Extrusion molding

    环保认证

    Environmental certification

    ROHS

    REACH

    EN71-3

    PAHS

    ASTM-F963

    Phthalate

    颜色Color

    透明Translucent

    气味Smell

    少许树脂味A little resin smell

    外型Appearance

    圆球形小颗粒Cylindrical particleabout 3mm×1.5mm

    储藏期Storage period

    常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months

    包装方式Packaging method

    25公斤/袋 25kg/bag

    物理性能Physical properties

    结果Result

    单位Unit

    方法Method

    成型条件Molding condition

    比重Specific gravity

    0.88±0.02

    g/cm3

    ASTM D792

    干燥温度Drying temp      

    硬度Hardness

    35±5

    shoreA

    ASTM D2240

    干燥时间Drying time     2Hours

    拉伸强度Tensile strength

    >2

    Mpa

    ASTM D412

    射嘴温度Nozzle temp     210

    断裂延伸Elongation at break

    >400

    %

    ASTM D412

    螺筒一段温度Screw 1 temp 200

    撕裂强度Tearing strength

    9

    Kn/m

    ASTM D624

    螺筒二段温度Screw 2 temp 190

    熔融指数Melt index

    25

    g/10min

    ASTM D1238

    螺筒三段温度Screw 3 temp 180

    常见包胶缺陷处理

      缺胶——提高加工注塑温度;增大注塑压力;改善材料流动性。

      劈缝,溢边——降低注塑温度;增大锁模力;减小注塑压力;从配方角度降低流动性。

      表面麻面,不光亮——提高注塑加工温度;烘料,减少原料水分。

      粘性差——注塑加工前充分烘料;提高注塑温度;调整配方。

      制品注塑变形——加强模具冷却;适当延长锁模时间。

      制品粘模——加脱模剂或润滑剂(对于内润滑剂——脱模剂应注意添加量,以防脱模剂析出

     