一米智能手表s1 智能手表手机超薄 R30B2-01

ER30B2-01是一款以SEBS和SBS混合的高分子材料,可快速成型。弹性好,耐磨。 ·ER30B2-01is a kind of polymer material which mixed SEBS and SBS which has high resilience and excellent wear resistance.Also it can be taken shape rapidly.   
  • 产品描述
  • 倍韧/BESTPERNE®ER30B2-01

    热塑性弹性体Thermoplastic Elastomer

    产品说明Product description

    ·ER30B2-01是一款以SEBSSBS混合的高分子材料,可快速成型。弹性好,耐磨。

    ·ER30B2-01is a kind of polymer material which mixed SEBS and SBS which has high resilience and excellent wear resistance.Also it can be taken shape rapidly.   

     

    关键特性Key characteristic

    1. 表面微亮,手感细腻A little bright on the surfaceexquisite touch
    2. 高回弹性High resilience
    3. 成型速度快,不粘模具Rapid moldingnon-stick mold

    4  耐磨,止滑性能好Excellent weather resistance and non-slip properties.

    功能Function

    产品应用

    Main application

    1 H电子产品HElectrical products

    3手把Handlebar

    2 H运动器材HSports equipment

    4玩具产品Toy products

    加工方法Processing method

     注塑成型Injection molding  挤出成型Extrusion molding

    环保认证

    Environmental certification

    ROHS

    REACH

    EN71-3

    PAHS

    ASTM-F963

    Phthalate

    颜色Color

    本色 Natural

    气味Smell

    少许树脂味A little resin smell

    外型Appearance

    圆球形小颗粒Cylindrical particleabout 3mm×1.5mm

    储藏期Storage period

    常温下通风干燥,24个月Ventilated dry at normal temperatureabout 24 months

    包装方式Packaging method

    25公斤/25kg/bag

    物理性能Physical properties

    结果Result

    单位Unit

    方法Method

    成型条件Molding condition

    比重Specific gravity

    0.92±0.02

    g/cm3

    ASTM D792

    干燥温度Drying temp      70

    硬度Hardness

    30±5

    shoreA

    ASTM D2240

    干燥时间Drying time     2Hours

    拉伸强度Tensile strength

    >2

    Mpa

    ASTM D412

    射嘴温度Nozzle temp     190

    断裂延伸Elongation at break

    >600

    %

    ASTM D412

    螺筒一段温度Screw 1 temp 180

    撕裂强度Tearing strength

    >9

    Kn/m

    ASTM D624

    螺筒二段温度Screw 2 temp 170

    熔融指数Melt index

    >16

    g/10min

    ASTM D1238

    螺筒三段温度Screw 3 temp 170

    设备方面

      (1)成型机合模力不足。如果成型机的额定合模力小于成型过程中制品从像投影面积上的张力,将会导致分型面间隙,造成飞边。

      解决方案:增大锁模力

      (2)成型机合模形成不足。如果成型机合模的最小间隙大于模具的厚度,制品的投影面积超过了注压机的最大注射面积,注压机模板安装调节不正确,模具安装不正确,锁模力不能保持恒定,注压机模板不平行,拉杆变形不均将会导致模具合模不紧密造成飞边。
     

     